Fixing up of welding defects in Locomotives

























In the light of RDSO’s letter , support lugs of Aluminium gearcase in the WAP 5 loco were inspected in the shop .






Welding defects in the WAG7 loco #28243 were pointed out to production staff in the testing shed. This loco was  due to be dispatched tomorrow and wedling defects were rectified.




Another welding defect in the compressor of WAP 4 loco #31333 was asked to be attended by production staff. This loco has light passing from roof section and was being attended in the test shed as due for dispatch .